I did the following:
1) using the 2 mm Sand (1.5 kg) for the crushers
2)
3 round 600) opened the gates, spilled out of the sand and bi
4) using a vacuum cleaner, clean grinding Chamber suction
5) using a cloth wipe the grinding balls 6.
) Dropped balls into the left Chamber (in proportion)
7) levels 96%
8) stir them in containers
9) For the crushing cans.
10) Turning 700 ring
11) open the gates and took 5 points
12) blended sample and check the Blaine, R45 R90
13) Go to 700 round.
14)